DIN 1.4021 pelat baja tahan karat
dapatkan harga terbaruJenis pembayaran: | L/C,T/T,D/P,D/A,Paypal,Others |
Min. Memesan: | 5 Ton |
Transportasi: | Ocean,Land,Air,Express |
Pelabuhan: | Shanghai Port,Tianjin Port,Qingdao Port |
Jenis pembayaran: | L/C,T/T,D/P,D/A,Paypal,Others |
Min. Memesan: | 5 Ton |
Transportasi: | Ocean,Land,Air,Express |
Pelabuhan: | Shanghai Port,Tianjin Port,Qingdao Port |
Bahan: 2B, 600 Seri, 300 Seri, 500 Seri, 200 Seri, 400 Seri
Standar: JIS, AiSi, ASTM, GB, KERIUHAN, EN
Tempat Asal: Cina
Jenis: Gulungan, Piring
Sertifikasi: RoHS, ISO, IBR, BV, Sgs
Toleransi: ± 1%
Layanan Pengolahan: Pembengkokan, Pengelasan, Dekorasi, Meninju, Pemotongan
Technique: Cold Rolled Hot Rolled
Surface: BA/2B/NO.1/NO.3/NO.4/8K/HL/2D/1D
Material: 201,202,301,302,303,304,304L,304N1,309S,310S,316,316L,316Ti,316N,317,317L,321,409L,410,420,430,904,904L,etc
Sample: Provided
Ketebalan: 0.2~6mm
Width: 1000~2000mm
Standar: GB, JIS, ASTM, AISI
Nilai: 200/300/400/500/600/700/800/900 series/duplex stainless steel
Menjual unit | : | Ton |
Tipe paket | : | Kemasan standar industri atau sesuai dengan persyaratan klien |
Contoh pada gamba | : |
The file is encrypted. Please fill in the following information to continue accessing it
DIN 1.4021 Stainless Steel Plate adalah stainless steel martensit yang mengandung kromium dan karbon. Ia juga dikenal sebagai X20CR13 atau AISI 420. Tingkat stainless steel ini memiliki ketahanan korosi yang baik, kekerasan tinggi, dan ketahanan aus yang baik. Ini biasanya digunakan dalam pembuatan pisau, gunting, instrumen bedah, dan alat pemotong lainnya. Komposisi kimia pelat baja stainless DIN 1.4021 adalah sebagai berikut:
- Karbon (C): 0,16-0,25%
- Chromium (CR): 12.0-14.0%
- Mangan (MN): 1,0% maks
- Fosfor (P): 0,04% maks
- Sulfur: 0,03% maks
- Silikon (SI): 1,0% maks
Sifat mekanis DIN 1.4021 pelat baja stainless adalah:
- Kekuatan tarik: 650-900 MPa
- Kekuatan Yield: 450-600 MPa
- Perpanjangan: 14-20%
- Kekerasan: 200-300 HBW
DIN 1.4021 Pelat baja tahan karat tersedia dalam berbagai ukuran dan ketebalan. Ini dapat dipasok dalam kondisi anil, dikeraskan, atau marah. Surface finish bisa cerah, dipoles, atau satin.
Komponen kimia lembaran stainless steel
Grade | C | Si | Mn | P | S | Ni | Cr | Mo |
201 | ≤0.15 | ≤0.75 | 5.5-7.5 | ≤0.06 | ≤0.03 | 3.5-5.5 | 16.0-18.0 | - |
202 | ≤0.15 | ≤1.0 | 7.5-10.0 | ≤0.06 | ≤0.03 | 4.-6.0 | 17.0-19.0 | - |
301 | ≤0.15 | ≤1.0 | ≤2.0 | ≤0.045 | ≤0.03 | 6.0-8.0 | 16.0-18.0 | - |
302 | ≤0.15 | ≤1.0 | ≤2.0 | ≤0.035 | ≤0.03 | 8.0-10.0 | 17.0-19.0 | - |
304 | ≤0.08 | ≤1.0 | ≤2.0 | ≤0.045 | ≤0.03 | 8.0-10.5 | 18.0-20.0 | |
304L | ≤0.03 | ≤1.0 | ≤2.0 | ≤0.035 | ≤0.03 | 9.0-13.0 | 18.0-20.0 | |
309S | ≤0.08 | ≤1.0 | ≤2.0 | ≤0.045 | ≤0.03 | 12.0-15.0 | 22.0-24.0 | |
310S | ≤0.08 | ≤1.5 | ≤2.0 | ≤0.035 | ≤0.03 | 19.0-22.0 | 24.0-26.0 | |
316 | ≤0.08 | ≤1.0 | ≤2.0 | ≤0.045 | ≤0.03 | 10.0-14.0 | 16.0-18.0 | 2.0-3.0 |
316L | ≤0.03 | ≤1.0 | ≤2.0 | ≤0.045 | ≤0.03 | 12.0-15.0 | 16.0-18.0 | 2.0-3.0 |
321 | ≤0.08 | ≤1.0 | ≤2.0 | ≤0.035 | ≤0.03 | 9.0-13.0 | 17.0-19.0 | - |
410 | ≤0.15 | ≤1.0 | ≤1.0 | ≤0.035 | ≤0.03 | - | 11.5-13.5 | - |
430 | 0.12 | ≤0.75 | ≤1.0 | ≤0.040 | ≤0.03 | ≤0.60 | 16.0-18.0 | - |
904L | ≤2.0 | ≤0.045 | ≤1.0 | ≤0.035 | - | 23.0-28.0 | 19.0-23.0 | 4.0-5.0 |